Standard
Reference standard:JIS Z 8901
*Material used:KANTO ( Japanese ) loam *Sintered at 800°C, 2hours.
*Particle density:2.9~3.1g/cm3
*Chemical composition
Chemical composition | % ( mass ) |
SiO2 | 34~40 |
Fe2O3 | 17~23 |
AI2O3 | 26~32 |
CaO | 0~3 |
MgO | 0~7 |
TiO2 | 0~4 |
Ignition Loss | 0~4 |
*Particle size distribution
Particle size µm |
Oversize(mass basis)% | ||
Class 7 | Class 8 | Class 11 | |
1 | – | 65±5 | |
2 | – | 50±5 | |
4 | – | 22±3 | |
5 | 88±5 | 61±5 | – |
6 | – | 8±3 | |
8 | – | 3±3 | |
10 | 76±3 | 43±3 | – |
20 | 62±3 | 27±3 | – |
30 | 50±3 | 15±3 | – |
40 | 39±3 | 9±3 | – |
75 | 20 max. | 3 max. |
Microscopic Photograph

Test Powders 1-Class7(KANTO(Japanese) loam )

Test Powders 1-Class8(KANTO(Japanese) loam )

Test Powders 1-Class11(KANTO(Japanese) loam )
Price