Summary

APPIE distributes the test powders SAP test powder 3 which are based on SAP 14-12(APPIE Standard).
SAP test powders 3 has smaller size distribution compared to the JIS Z 8901 Test powders 1, and they can be used for the performance test of various dust collectors and air filters as well as for durability test of various instruments when they are exposed to dust particles.

SAP Test Powders 3 Class 1 ( STP3-1 ) ( Quartz sand )

Material: Quarts sand

particle density : 2.6∼2.7 g/cm3

Chemical component

Chemical component % ( weight )
SiO2 95 (min.)
Fe2O3 5 (max.)
AI2O3
TiO2
MgO
Ignition Loss

 

Particle size distribution – measured by Laser Diffraction-Scattering Method

Undersize (volume%) Particle size range ( µm )
10 0.75~1.1
20 1.1~1.7
30 1.3~2.0
40 1.5~2.3
50 1.7~2.6
60 1.9~2.8
70 2.0~3.0
80 2.3~3.4
90 2.8~4.1

 

Electron Microscopic Photograph

SAP test powders 3, Class 1 (Quartz sand)

SAP test powders 3, Class 1 (Quartz sand)

SAP Test Powders 3 Class 2 ( STP3-2 ) ( Talc )

Material: Talc

particle density : 2.7∼2.9 g/cm3

Chemical component

Chemical component % ( weight )
SiO2 60∼63
Fe2O3 0∼3
AI2O3 0∼3
CaO 0∼2
MgO 30∼34
Ignition Loss 3∼7

 

Particle size distribution – measured by Laser Diffraction-Scattering Method

Undersize (volume%) Particle size range ( µm )
10 1.7~2.9
20 2.3~3.9
30 2.7~4.6
40 3.1~5.3
50 3.6~6.1
60 4.0~6.9
70 4.4~7.6
80 5.1~8.7
90 6.3~11

 

Electron Microscopic Photograph

SAP test powders 3, Class 2 (Talc)

SAP test powders 3, Class 2 (Talc)

SAP Test Powders 3 Class 3 ( STP3-3 ) ( Sintered KANTO loam )

Material: Sintered KANTO loam

particle density : 2.9∼3.1 g/cm3

Chemical component

Chemical component % ( weight )
SiO2 34∼40
Fe2O3 17∼23
AI2O3 26∼32
CaO 0∼3
MgO 0∼7
TiO2 0∼4
Ignition Loss 0∼4

*Kanto Loam is natural soil and the ingredient may slightly vary according to the collection place.
 

Particle size distribution – measured by Laser Diffraction-Scattering Method

Undersize (volume%) Particle size range ( µm )
10 0.89~1.3
20 1.2~1.7
30 1.4~2.0
40 1.5~2.3
50 1.7~2.5
60 1.8~2.7
70 2.0~2.9
80 2.4~3.5
90 2.9~4.2

 

Electron Microscopic Photograph

SAP test powders 3, Class 3 (Sintered KANTO Loam)

SAP test powders 3, Class 3 (Sintered KANTO Loam)

SAP Test Powders 3 Class 4 ( STP3-4 ) ( Calcium carbonate (ground) )

Material: Calcium carbonate (ground)

particle density : 2.7∼2.8 g/cm3

Chemical component

Chemical component % ( weight )
CaO 54∼56
MgO 0∼3
SiO2 0∼4
AI2O3 0∼3
Fe2O3 0∼1
Ignition Loss 42∼45

 

Particle size distribution – measured by Laser Diffraction-Scattering Method

Undersize (volume%) Particle size range ( µm )
10 0.31~0.54
20 0.38~0.65
30 0.45~0.79
40 0.57~0.97
50 0.75~1.3
60 0.95~1.7
70 1.2~2.0
80 1.4~2.4
90 1.7~3.0

 

Electron Microscopic Photograph

SAP test powders 3, Class 4 (Calcium carbonate (ground))

SAP test powders 3, Class 4 (Calcium carbonate (ground))

Product Price

Classification Package (kg) Price

( JPY )
SAP test powders 3, Class 1 ( STP3-1 )
( Quartz sand )
1.5 23,000
SAP test powders 3, Class 2 ( STP3-2 )
(Talc )
1.0 14,500
SAP test powders 3, Class 3 ( STP3-3 )
(Sintered KANTO loam )
2.0 24,300
SAP test powders 3, Class 4 ( STP3-4 )
( Calcium carbonate (ground) )
1.5 14,500

(2023.1.1)

 